Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | |
ND Industries 542 Shaft & Bearing Retainer Retaining Compound Very high strength retainer for gears, wheels, pulleys, fans, cams, collars, flywheels, rotors to shaftMeets military spec Mil-R-46082B Type III |
|||
Viscosity | 1600 - 2500 cP | 1600 - 2500 cP | |
ND Industries High Temperature SuperGlue 362 Medium viscosity with thermal cycling resistance |
|||
Viscosity | 2300 - 2500 cP @Temperature 23.0 °C |
2300 - 2500 cP @Temperature 73.4 °F |
|
Prodways PLASTCure Model 300 3D Printing Polymer Good mechanical properties.Broad range of dental model applications.Information provided by Genistar. |
|||
Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
Palm Labs Adhesives Turbo Fuse Series 180 (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performanc.. |
|||
Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 180 BLACK TOUGHENED (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 143 – BLACK TOUGHENED advanced formula is designed to polymerize instantly by absorbing surface moisture. The p.. |
|||
Viscosity | 2300 - 2500 cP | 2300 - 2500 cP | Liquid State |
Palm Labs Adhesives TURBO FUSE SERIES 180 MEDICAL DEVICES APPROVED (2400 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 180 - MEDICAL DEVICES APPROVED advanced formula is designed to polymerize instantly by absorbing surface moistur.. |
|||
Viscosity | 1200 - 2500 cP @Temperature 25.0 °C |
1200 - 2500 cP @Temperature 77.0 °F |
Uncured |
Permabond 240 Cyanoacrylate, gap filling PERMABOND® 240 is a high viscosity product useful in large gap applications. It is ideal for porous substrates. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate.. |
|||
Viscosity | 2100 - 2500 cP | 2100 - 2500 cP | |
Huntsman Araldite GY 9613 Bisphenol A Epoxy Liquid Resin Weight per Epoxide (EEW, g/eq) 188 to 197. Max color is 1.Comments/Applications: GY 2600 modified with DY 025 (Epoxide 8). Very light color. High solids and solvent free coatings and floorings.Da.. |
|||
Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
Huntsman HY 356 Aliphatic Amine Mix Ratio with GY 6010 is 35.Comments/Applications: A medium viscosity phenol free aliphatic amine adduct. Industrial maintenance, coatings, tank lining, pipe coatings and flooring.Data provided b.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2061027P15 High Brightness Phosphor Ink (Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2070126P5 High Brightness Phosphor Ink (White) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 1500 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
1500 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2070209P5 High Brightness Phosphor Ink (Green) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2080211P2 High Brightness Phosphor Ink (Blue/Green & Blue) This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 2100 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
2100 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials R2040212D3 High Viscosity Acrylic Pressure Adhesive for Diagnostic Sensors This material has a high viscosity, it is a water based acrylic pressure sensitive screen printable adhesive. It can be used in many different diagnostic applications such as test cards, assays and.. |
|||
Viscosity | 860 - 2500 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
860 - 2500 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials C2101125P4 High Brightness Phosphor Ink This product is part of a range of Heat Curable Inks designed specifically for use in Electro Luminescent systems. These products are based on a unique curing process that results in the low tempera.. |
|||
Viscosity | 1100 - 2500 cP @Time 7200 sec |
1100 - 2500 cP @Time 2.00 hour |
V-170-0 |
Solvay JAGUAR® HP 120 Surfactant Description: Best suited for use with solvents, even 100% ethanol based formulations. Jaguar HP 120 is a natural thickener and film former for hand sanitizersChemical Name: HYDROXYPROPYL GUARC.T.F.A.. |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | #3 SP, 12 rpm; RP-1234 |
Solvay MIRACARE® MS-2 Surfactant Description: Formulated surfactant concentrate that is readily dilutable to yield ultra-mild cleansing products. Low eye and skin irritation.Chemical Name: AMPHOTERIC/ANIONIC/NONIONIC SURFACE ACTIVE.. |
|||
Viscosity | 1000 - 2500 cP @Temperature 125 °C |
1000 - 2500 cP @Temperature 257 °F |
V-005 |
Westlake Epolene® EE-2 Emulsifiable - Oxidized Low Molecular Weight Polyethylene Polymer Product Description: EE-2 is a medium density, low molecular-weight oxidized polyethylene with exceptional hardness. It is an excellent asphalt modifier which mixes readily with all asphalts. It h.. |
|||
Viscosity | 300 - 2500 cP | 300 - 2500 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy.. |
|||
Viscosity | 500 - 2500 cP | 500 - 2500 cP | Milled Cement; Zeon Test #327 |
Zeon Chemicals Nipol® 1031 Nitrile Elastomer Nipol 1031 is a copolymer of butadiene and acrylonitrile with very high oil resistance. Sufficient non-staining antioxidant is added during manufacture for normal storage conditions.Excellent fuel a.. |
|||
Viscosity | 1800 - 2500 cP | 1800 - 2500 cP | Part A |
Master Bond EP21LSCL-1 Two Component, Room Temperature Curing Epoxy Resin Product Description: Master Bond Polymer System EP21LSCL-1 is a two component, low viscosity epoxy resin system featuring optical clarity as well as non-yellowing properties. This system can be used.. |
|||
Viscosity | 2100 - 2500 cP @Temperature 23.0 °C |
2100 - 2500 cP @Temperature 73.4 °F |
|
Master Bond EP27 Low Temperature Curing Two Component Epoxy Master Bond Polymer System EP27 is a unique two component
epoxy formulation offers relatively fast cures at temperatures as low as 40°F and below, with curing times much shorter than currently exis.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 23.0 °C |
1500 - 2500 cP @Temperature 73.4 °F |
|
Master Bond UV15-7DC One Component, Dual Cure UV System Master Bond UV15-7DC is a one component, dual cure UV system for high performance bonding, sealing, coating and encapsulation applications. This system features a primary cure utilizing UV light and.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 23.0 °C |
1500 - 2500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OE101 Two Component Epoxy Material Description: A two component epoxy designed for low stress applications in fiber optic packaging, opto-electronics and semiconductors. It is a lower modulus version of EPO-TEK® 353ND.Inf.. |
|||
Viscosity | 1500 - 2500 cP | 1500 - 2500 cP | MA143LFE |
C.O.I.M. FILCO® 309 Film Former for Glass Fiber Sizes Description: Film Former for Glass Fiber SizesGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and ar.. |
|||
Viscosity | 1500 - 2500 cP @Temperature 35.0 °C |
1500 - 2500 cP @Temperature 95.0 °F |
|
C.O.I.M. UREXTER® T 404 Polyurethane Two-Component Compound Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc. |
|||
Viscosity | 1000 - 2500 cP | 1000 - 2500 cP | |
Aremco Graphi-Coat™ 623 High Temperature Specialty Coatings Inorganic, Titanium Diboride Filled This coating system, originally patented by Aremco, is a tow-part, silica-bonded, titanium diboride filled, oxidation resistant coating for protecting graphite from oxidation to 2000°F (1093°C). U.. |
|||
Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
Aremco Cerama-Dip™ 538-N High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
Aremco Cerama-Dip™ 538-N-BLK High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |
|||
Viscosity | 2000 - 2500 cP | 2000 - 2500 cP | Brooksfield LV Viscometer |
Aremco Cerama-Dip™ 538-N-GRN High Temperature Specialty Ceramic-Inorganic Coating Low viscosity, light gray coating for powder resistors and rheostats to 2600°F (1427°C). black and green pigments also available. |