Huntsman AroCy XU 371 Semi-Solid Resin

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name AroCy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman AroCy XU 371 Semi-Solid Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Comments/Applications: Trifunctional semi-solid resin. Applications include composites, adhesives and sealers requiring mechanical strength at temperatures (non-continuous) as high as 300°C.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 300 - 600 cP
300 - 600 cP