Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300 - 500 cP | 300 - 500 cP | |
ND Industries 388 Toughened Instant Superglue Black toughened Cyanoacrylate for metal, rubber, and plastic |
|||
Viscosity | 300 - 900 cP @Temperature 25.0 °C |
300 - 900 cP @Temperature 77.0 °F |
|
Northstar Polymers PPA-017 Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 300 cP | 300 cP | Part B, RVT, #2, 20 rpm; TM R050-12 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Viscosity | 300 cP | 300 cP | |
Resinlab® CYNERGY CA6501 Adhesive Description: The CYNERGY 6500 SERIES are black, highly toughened, high peel strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. They impa.. |
|||
Viscosity | 300 - 600 cP | 300 - 600 cP | |
Huntsman AroCy XU 371 Semi-Solid Resin Comments/Applications: Trifunctional semi-solid resin. Applications include composites, adhesives and sealers requiring mechanical strength at temperatures (non-continuous) as high as 300°C.Data.. |
|||
Viscosity | <= 300 cP | <= 300 cP | |
Solvay Specialty Polymers Solvera® PT 5060 PFPE Surface Treatment Solvera® PFPE is a sustainable surface treatment developed to increase the grease resistance of paper packaging, pizza boxes, popcorn bags, pet food bags and food wraps. Both solvent and aqueous.. |
|||
Viscosity | <= 300 cP @Temperature 40.0 °C |
<= 300 cP @Temperature 104 °F |
#3 sp. @ 5 RPM; RP-0596 |
Solvay GEROPON® T-22 A Surfactant Identification: AQUEOUS SOLUTION OF SURFACTANT SALTCAS: 137-20-2Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: GEROPON T-22/A is a N-methyl oleyl taurate, useful as.. |
|||
Viscosity | 300 - 400 cP | 300 - 400 cP | Part B |
Master Bond EP30AN-1 Low Viscosity, NASA Low Outgassing Epoxy Description: Master Bond EP30AN-1 is a two part epoxy for high performance potting, sealing, coating and bonding featuring high thermal conductivity, excellent electrical insulation properties and N.. |
|||
Viscosity | 300 - 400 cP @Temperature 23.0 °C |
300 - 400 cP @Temperature 73.4 °F |
|
Master Bond EP37-3 Optically Clear, Impact Resistant Two Component Epoxy Master Bond Polymer System EP37-3 is a low viscosity, resilient, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. As an adhes.. |
|||
Viscosity | 300 cP @Temperature 200 °C |
300 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3215 Polyester, Pellet Low molecular weight type UE3210UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink bin.. |
|||
Viscosity | 300 cP @Temperature 200 °C |
300 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3240 Polyester, Pellet Medium Tg high elongation, Binder paint, Adhesive agentUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adh.. |
|||
Viscosity | 300 - 2500 cP | 300 - 2500 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals HyTemp® 4051CG AR Polyacrylate Elastomer HyTemp 4051CG contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat and compression set resistance.Cement grade version of Hy.. |
|||
Viscosity | 300 - 2700 cP | 300 - 2700 cP | Unmilled Cement; Zeon Test #328 |
Zeon Chemicals HyTemp® 4051CG Polyacrylate Curative HyTemp 4451CG is a ground form of HyTemp 4051CG, which contains one or more acrylic esters with a small percentage of a carboxy/chlorine cure site.Contains acrylic esters with a small percentage of .. |
|||
Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2113 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to gla.. |
|||
Viscosity | 300 cP @Temperature 25.0 °C |
300 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 931-1 Low Viscosity Encapsulant TRA-BOND 931-1 low viscosity epoxy encapsulant is designed for high reliability applications, where capillary action is desired. This encapsulant provides environmental and mechanical protection.Inf.. |
|||
Viscosity | 300 cP @Temperature 23.0 °C |
300 cP @Temperature 73.4 °F |
|
Master Bond UV19 One Component, Low Viscosity, Optically Clear UV Curable System Master Bond Polymer System UV19 is a newly developed UV curable, low viscosity optically clear compound specifically designed for high performance laminating, sealing, bonding and coating. This acry.. |
|||
Viscosity | 300 cP @Temperature 200 °C |
300 cP @Temperature 392 °F |
Melt |
Unitika elitel UE3216 Polyester, Pellet Low Tg type UE3215UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders, and modi.. |
|||
Viscosity | 300 cP | 300 cP | dynamic |
Dow Corning SYL-OFF® SL 3000 CATALYST 1,000 ppm platinum in vinyl polymerInformation provided by Dow Corning |
|||
Viscosity | 300 cP @Temperature 30.0 °C |
300 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC +3 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Viscosity | 300 cP @Temperature 30.0 °C |
300 cP @Temperature 86.0 °F |
|
DSM Somos® ProtoGen™ O-XT 18120 Epoxy Resin for Stereolithography, UV Postcure at HOC -2 DescriptionDSM Somos® ProtoGen O-XT 18120 is a liquid photopolymer that produces accurate parts ideal for general purpose applications. ProtoGen resins are the first SL resins to demonstrate diffe.. |
|||
Viscosity | 300 - 500 cP @Temperature 23.0 °C |
300 - 500 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OE121 Black Epoxy Adhesive Material Description: A two component, low temperature curing epoxy adhesive designed for semiconductor flip chip underfill. It is color coded black for visual ID during the underfilling process. .. |
|||
Viscosity | 300 - 600 cP @Temperature 23.0 °C |
300 - 600 cP @Temperature 73.4 °F |
100 rpm |
Epoxy Technology EPO-TEK® OG178 UV Cure Optical Epoxy Material Description: A single component, UV/visible shifted light curable epoxy, designed for adhesive, sealing, coating and encapsulating applications found in semiconductor, electro-optics, fiber.. |
|||
Viscosity | 300 - 600 cP | 300 - 600 cP | |
Epoxyset Epoxibond EB-109M-4 Unfilled Epoxy Adhesive A two-component, unfilled, flexible epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries. EB-109M-4 puts low stress on fragile parts a.. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 400 cP | 300 - 400 cP | |
Aremco Lamp-Coat™ LC4010-GL High Temperature Coating, Silicone Aluminum-filled coating for application directly over uncoated headlamps to 1020 ºF (550 ºC) |
|||
Viscosity | 300 - 400 cP | 300 - 400 cP | |
BASF Lupranate® 277 Isocyanate Description: Lupranate® 277 Isocyanate is a medium viscosity polymeric MDI isocyanateInformation provided by BASF |
|||
Viscosity | 300 cP | 300 cP | Part B, RVT, #3, 2.5 rpm; TM R050-12 |
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate .. |
|||
Viscosity | 300 cP | 300 cP | |
Loctite® 480 Toughened Ethyl Cyanoacrylate Bonding Adhesive Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-.. |