Material Notes:
Mix Ratio with 100 phr GT 70130 is 6.Comments/Applications: Solid resinous amino-containing hardener. *Mix ratio with Araldite GT 7013. For low temperature cure, high gloss. Decorative and protective powder coatings.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 - 100 °C
194 - 212 °F
Softening Range
Processing Properties Metric English Comments
Processing Temperature 120 °C
248 °F
Cure Schedule: 15 min @ 120°C