Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 60.0 - 100 °C | 140 - 212 °F | Average value: 84.3 °C Grade Count:5 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Extruded". Each property range of values reported is minimum and .. |
|||
Maximum Service Temperature, Air | 70.0 - 100 °C | 158 - 212 °F | Average value: 80.0 °C Grade Count:3 |
Overview of materials for Polycarbonate, Optical Grade This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a.. |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | Softening Range |
Huntsman HT 3261 Special Hardener Mix Ratio with 100 phr GT 70130 is 6.Comments/Applications: Solid resinous amino-containing hardener. *Mix ratio with Araldite GT 7013. For low temperature cure, high gloss. Decorative and prote.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® AS/2 PA66 Product description: Grilon AS/2 is an unreinforced PA66 injection molding grade. Grilon AS/2 has the following important properties: Good flow behaviorEasy processingShort cycle times Grilon AS/2 i.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® BG-30 EC PA6-GF30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® BG-40 HM PA6-GF40 Product description: Grilon BG-40 HM is a heat stabilized, normal viscosity, and adhesion modified PA6 injection molding grade with 40% glass fibers. Grilon BG-40 HM has the following important prop.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® BT 40 Z PA6 Product description: Grilon BT 40 Z is an unreinforced, normal viscosity, impact modified polyamide blend with amorphous and semi-crystalline components. Grilon BT 40 Z has the following important p.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® BZ 3 PA6 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 20 G grey 9280 PA12 Product Description: Grilamid L 20 G grey 9280 is a medium viscosity, unreinforced, heat stabilized polyamide 12 for injection molding and cable sheathing. The main features of this product are: Low.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 20 nat PA12 Medium viscosity unmodified Polyamide 12Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 20 W 20 PA12 Product Description: Grilamid L 20 W 20 is a semi-flexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 is heat stabilized. The main features of Grilamid L 20.. |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 20H FWA black 9225 PA12 Product Description Grilamid L 20 H FWA black 9225 is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA black 9225 is used for technical injection molded .. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TR 30 nat PA* Product description: Grilamid TR 30 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 natural offers outstanding properties.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TR 90 PAMACM12 Product description: Grilamid TR 90 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 natural offers outstanding properties.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TSS/4 LF 2 PA666 Product description: Grilon TSS/4 LF 2 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 2% lubricant (molybdenum disulphide). Grilon TSS/4 LF 2 has the following import.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TSZ 3 PA666 Product description: Grilon TSZ 3 is a heat stabilized, normal viscosity, high impact modified PA66 + PA6 injection molding grade. Grilon TSZ 3 has the following important properties: Excellent toug.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® XE 3841 nat PA12 Product description: Grilamid XE 3841 is a flexible, heat stabilized and plasticizer-free Polyamide 12, which offers a very good processability for extrusion. Grilamid XE 3841 is qualified in Europe.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® XE 3997 nat PAMACM12 Product description: Grilamid XE 3997 natural is a transparent thermoplastic polyamide based on aliphatic and cycloaliphatic blocks. Grilamid XE 3997 natural is particularly suitable for blow molded.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® XE 4028 nat PA12/MACMI Product description: Grilamid XE 4028 natural is a transparent thermoplastic polyamides based on aliphatic, cycloaliphatic and aromatic blocks. Grilamid XE 4028 natural offers a variety of interesti.. |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® XE 4158 nat PA612 Product description: Grilamid XE 4158 natural is a medium viscosity Polyamide 12 with super high impact strength. The main features of Grilamid XE 4158 natural are: Very good hydrolysis resistanceGo.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® BK-30 PA6-GB30 Information provided by EMS Grivory |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 20H FWA nat PA12 Product Description: Grilamid L 20 H FWA natural is a medium viscosity, unreinforced and heat stabilized Polyamide 12 (PA12). Grilamid L 20 H FWA natural is used for technical injection molded parts.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 25 W 40 PA12 Product Description: Grilamid L 25 W 40 is a flexible, plasticised, high viscosity extrusion grade of Polyamide 12 (PA12) Grilamid L 25 W 40 is UV and heat stabilized. The main features of Grilamid .. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TR 55 PA12/MACMI Product description: Grilamid TR 55 natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 55 natural offers outstanding properties.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TR 90 LS PAMACM12 Product description: Grilamid TR 90 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 90 LS natural contains a processing a.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | long term; EMS |
EMS-Grivory Grivory® TR 90 NZ PAMACM12-I Product description: Grilamid TR grades are transparent thermoplastic polyamides based on aliphatic and cycloaliphatic blocks. Grilamid TR 90 NZ offers a variety of interesting properties such as: o.. |
|||
Maximum Service Temperature, Air | 80.0 - 100 °C | 176 - 212 °F | Long Term |
CENTROPLAST CENTROMID 12 LE soft Polyamide 12 LE soft This extruded material is suitable for conveying foodstuffs and pharmaceutical products. It is used in flexible tubes for worm gears and spiral conveyors.Information provided by CENTROPLAST Enginee.. |
|||
Maximum Service Temperature, Air | 40.0 - 100 °C | 104 - 212 °F | Average value: 52.4 °C Grade Count:30 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |
|||
Maximum Service Temperature, Air | 90.0 - 100 °C | 194 - 212 °F | long term; EMS |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |