Material Notes:
Mix Ratio with GY 6010 is 35.Comments/Applications: Finely ground HT 939. Adhesives, tooling, vinyl plastisols, dipping compounds.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Softening Point
Processing Properties Metric English Comments
Processing Temperature 150 °C
302 °F
Cure Schedule: 6.5 min @ 150°C