Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Processing Temperature = 150 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Processing Temperature 150 - 210 °C
302 - 410 °F
PolyChem Alloy GMS 2004D Foam Stabilizer
PE Foam Stabilizer
Processing Temperature 150 °C
302 °F
Compression or Injection Molding
Premix Premi-Glas® 1100-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100-20 is a fiberglass reinforced thermoset bulk molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent sti..
Processing Temperature 150 °C
302 °F
Compression or Injection Molding
Premix Premi-Glas® 1100V-20 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-20 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 1200-15 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-15 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 1200H-20 Polyester SMC
Premi-Glas® 1200H-20 is a 20% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where good arc resistance and dielectric strength are required and UL 94HB flame rec..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 1203-30 Fiberglass Reinforced SMC
Description: Premi-Glas® 1203-30 is a fiberglass-reinforced, thermoset sheet molding compound designed for structural and semi-structural components where smooth flat surfaces, high strength and st..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 1205 Glass Reinforced SMC
Description: Premi-Glas® 1205 is a glass reinforced thermoset Sheet Molding Compound formulated for residential door skins and similar construction applications. Key features and benefits: Excellen..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2200-15 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-15 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2200-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2203-22 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Processing Temperature 150 - 170 °C
302 - 338 °F
Collar Temperature
Solvay Specialty Polymers Cogegum® AFR/720 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Processing Temperature 150 - 170 °C
302 - 338 °F
Collar Temperature
Solvay Specialty Polymers Cogegum® AFR/760 Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Processing Temperature 150 - 170 °C
302 - 338 °F
Collar Temperature
Solvay Specialty Polymers Cogegum® AFR/765-UV Polyolefin, Unspecified  (Unverified Data**)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Processing Temperature 150 °C
302 °F
Compression Molding
Premix Premi-Glas® 1281-47 VE SMC
Description: Premi-Glas® 1281-47 VE is a sheet molding compound.Market: StructuralInformation provided by Premix.
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
Lucobit Lucofin® 1410 Polyolefin TPO Granules, Grey
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Processing Temperature 150 - 200 °C
302 - 392 °F
Profiles
Lucobit Lucolit® 1323 Polyolefin TPO Granules, Green
Lucolit is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucolit products display excellent tear resistance, flexibility, and weathering resistance. Lucolit exhi..
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
Lucobit Lucobit® 1233 Ethylene Copolymer Bitumen
Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of speci..
Processing Temperature 150 - 180 °C
302 - 356 °F
Total EVA 1010 VN 3 Ethylene Vinyl Acetate Copolymer - Blown Film
EVA 1010 VN 3 is made by a high pressure tubular process. Grade for films with high transparency and high mechanical properties. Contains an antioxidant.Application examples: Stretch film, food pa..
Processing Temperature 150 - 190 °C
302 - 374 °F
Total LDPE 1022 FH 24 Low Density Polyethylene - Blown Film
LDPE 1022 FH 24 is a low density polyethylene made by a high pressure process.LDPE 1022 FH 24 is a slip and anti-block formulated grade.LDPE 1022 FH 24 is suited to many applications in the field of..
Processing Temperature 150 - 190 °C
302 - 374 °F
Films Die Head
EMS-Griltech Griltex® D 1439E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Processing Temperature 150 - 190 °C
302 - 374 °F
Films Die Head
EMS-Griltech Griltex® D 1519E Copolyester Hotmelt Adhesive (Technical Applications)
Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo..
Processing Temperature 150 °C
302 °F
Cure 0.25 hrs
Aptek 2710A/B Low modulus silicone adhesive
Low modulus silicone adhesive; -110ºC to 260ºC operating range; Low outgassing/space grade; Electrostatically Discharging (ESD)APTEK 2710-A/B is a two component, black, low modulus, thixotropic, s..
Processing Temperature 150 - 165 °C
302 - 329 °F
Mixture Zone
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
Lucobit Lucofin® 1410MB Polyolefin TPO Granules, Grey
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
Lucobit Lucofin® 1460 Polyolefin TPO Granules, White
Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi..