Material Notes:
Mix Ratio with GY 6010 is 35.Comments/Applications: A medium viscosity phenol free aliphatic amine adduct. Industrial maintenance, coatings, tank lining, pipe coatings and flooring.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 1000 - 2500 cP
1000 - 2500 cP
Processing Properties Metric English Comments
Pot Life 20 min
20 min