Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Huntsman Corporation
Trade Name IROGRAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
ASTM D792
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D995
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 54.0 MPa
7830 psi
DIN 53504
Elongation at Break 610 %
610 %
ASTM D412
100% Modulus 0.0204 GPa
2.96 ksi
DIN 53504
300% Modulus 0.0326 GPa
4.73 ksi
DIN 53504
Rebound 34 %
34 %
Bayshore; ASTM D2632
Tear Strength 219 kN/m
1250 pli
ASTM D624
Abrasion 30
30
[mm<sup>3</sup>]; ISO 4649
Compression Set 44 %

@Temperature 23.0 °C,
Time 252000 sec
44 %

@Temperature 73.4 °F,
Time 70.0 hour
ASTM D395
56 %

@Temperature 70.0 °C,
Time 86400 sec
56 %

@Temperature 158 °F,
Time 24.0 hour
ASTM D395
Thermal Properties Metric English Comments
Melting Point 205 - 215 °C
401 - 419 °F
Huntsman/TMA