Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 205 °C | 401 °F | ASTM D789 |
NYCOA 2011 Copolymer Nylon impact resistant, exceptional toughness and flexibility, flexible tubing & fishing lineInformation provided by NYCOA, Inc. |
|||
Melting Point | 205 °C | 401 °F | ISO METHOD 3146C |
NYCOA 2012 Copolymer Nylon easy flowing, exceptional toughness and flexibility with lower water absorptionInformation provided by NYCOA, Inc. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | Average value: 218 °C Grade Count:73 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Melting Point | 205 - 255 °C | 401 - 491 °F | Average value: 220 °C Grade Count:67 |
Overview of materials for Nylon 6, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Melting Point | 205 - 215 °C | 401 - 419 °F | Huntsman/TMA |
Huntsman IROGRAN® D 60 E 4024 Polyester-Based TPU-High Performance Grade High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman |
|||
Melting Point | 205 °C | 401 °F | Peak |
LG Chemical KEYFLEX BT 1055D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Melting Point | 205 °C | 401 °F | ISO R 1218 |
Schwartz Technical Plastics LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry Application: outrigger floats, rollersInformation provided by Schwartz Technical Plastics GmbH |
|||
Melting Point | 205 - 215 °C | 401 - 419 °F | |
Shandong Guangyin PA 612 Nylon Resin Features and Applications: As one kind of nylon with better tenacity, PA612 is mainly applicable to coating of high-grade toothbrush monofilaments, monofilaments and cables.Information provided by S.. |
|||
Melting Point | 205 °C | 401 °F | ASTM D3418 |
SK Chemicals SKYPEL G355D Special Grade Flexibility-Resistant Grade SKYPEL is a thermoplastic polyester elastomer (TPEE). It is a polymer resin having the property somewhere between plastics and rubber, which have various properties ranging from high hardness plasti.. |
|||
Melting Point | 205 °C | 401 °F | |
Zell-Metall Engineering Plastics Zellamid 1100 OIL Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Melting Point | 205 °C | 401 °F | |
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces .. |
|||
Melting Point | 205 °C | 401 °F | |
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads .. |
|||
Melting Point | 205 °C | 401 °F | Crystalline Peak; ASTM D3418 |
Eastman Eastman AP006 Copolyester Applications:Automotive componentsBreathable filmsElectrical/electronic componentsFilm ModificationFlexible hingesHose mandrelIndustrial componentsIndustrial hoses/beltsOffice furniturePackagingPoly.. |
|||
Melting Point | 205 °C | 401 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Neostar FN006 Elastomer Neostar FN006 elastomer is the second in Eastman’s series of tough, clear, durable copolyester ethers. Developed for use in the profile and automotive markets, it can also be used in packaging and .. |
|||
Melting Point | 205 °C | 401 °F | 10°C/min; ISO 11357-1/-3 |
DSM Novamid® 2620A PA6/6T Extrusion |
|||
Melting Point | <= 205 °C | <= 401 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 00309 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00309 is a copolymer of ethylene and vinyl acetate. Processing Conditions: Processing temperatures above 270°C (513°F) may cause resin degradation. Availability: Africa & M.. |
|||
Melting Point | <= 205 °C | <= 401 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ UL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00112 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applica.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Comtuf® 610 Nylon 6, Glass Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Comtuf® 651 Nylon 6, Mineral Reinforced, Impact Modified Data provided by the manufacturer, ComAlloy International Company.35% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i.. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 610 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 612 Nylon 6, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 614 Nylon 6, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.45% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 617 Nylon 6, Glass/Mineral Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.55% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Hiloy® 662 Nylon 6, Glass Bead Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Glass Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Melting Point | 205 - 225 °C | 401 - 437 °F | |
A. Schulman ComAlloy Lubrilon® 610 Nylon 6, Carbon Fiber/PTFE Reinforced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Melting Point | 205 °C | 401 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® CM551 TPC-ES Heat Resistant Copolyester |
|||
Melting Point | 205 °C | 401 °F | 10°C/min; ISO 11357-1/-3 |
DSM Arnitel® CM600-V TPC-ES FR Extrusion, Flame Retardant (Halogen free) |
|||
Melting Point | <= 205 °C | <= 401 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Escorene™ FL 00112 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00112 is a copolymer of ethylene and vinyl acetate offering low gel. Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No App.. |
|||
Melting Point | 205 °C | 401 °F | ASTM D2117 |
Samyang Triel® 5652EM Thermoplastics Polyetherester Elastomer, Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5652EM is an extrusion grade.Information provided by Samyang. |