Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film

Category Polymer , Film , Thermoplastic , Polyurethane, TP
Manufacturer Huntsman Corporation
Trade Name KRYSTALFLEX®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
ASTM D2240
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D412
Elongation at Break 550 %
550 %
ASTM D412
100% Modulus 0.00621 GPa
0.900 ksi
ASTM D412
300% Modulus 0.0124 GPa
1.80 ksi
ASTM D412
Tear Strength 78.9 kN/m
450 pli
ASTM D624
Peel Strength 21.2 kN/m

@Temperature 118 °C
121 pli

@Temperature 244 °F
resistance to glass with primer; ASTM D3167
26.3 kN/m

@Temperature 127 °C
150 pli

@Temperature 261 °F
resistance to glass with primer; ASTM D3167
Thermal Properties Metric English Comments
Glass Transition Temp, Tg -38.0 °C
-36.4 °F
Processing Properties Metric English Comments
Melt Temperature 85.0 - 120 °C
185 - 248 °F