Peel Strength 21.2 kN/m

@Temperature 118 °C
121 pli

@Temperature 244 °F
resistance to glass with primer; ASTM D3167
Huntsman KRYSTALFLEX® PE 192 Polyurethane Optical Aliphatic Film
Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers