Material Notes:
C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 7.0 g/10 min
7.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength, Yield 23.5 MPa
3410 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 0.686 GPa
99.6 ksi
ASTM D790
Izod Impact, Unnotched 0.735 J/cm
1.38 ft-lb/in
ASTM D256
Heat Seal Strength Initiation Temperature 125 °C
257 °F
Thermal Properties Metric English Comments
Melting Point 130 °C
266 °F
HS Method
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Users viewing this material also viewed the following: