Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.686 - 7.11 GPa | 99.6 - 1030 ksi | Average value: 2.10 GPa Grade Count:299 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Flexural Modulus | 0.686 GPa | 99.6 ksi | ASTM D790 |
Hyosung Topilene C600H PP C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.686 GPa | 99.6 ksi | ASTM D790 |
Hyosung Topilene C600HF PP C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 0.686 GPa @Thickness 6.40 mm |
99.6 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Flexural Modulus | 0.686 GPa @Thickness 3.20 mm |
99.6 ksi @Thickness 0.126 in |
ASTM D790 |
Supreme Petrochem SC 6501 Toughened Polystyrene Characteristics Excellent melt strength Extremely tough Easy printability Easy miscibility with most grades of polystyrene Processing Extrusion Thermoforming Injection MoldingApplications Impac.. |