Material Notes:
HJ646 Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 24.5 MPa
3560 psi
ASTM D638
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Izod Impact, Unnotched 1.96 J/cm
3.67 ft-lb/in
ASTM D256
0.686 J/cm

@Temperature -10.0 °C
1.29 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
257 °F
ASTM D648
Users viewing this material also viewed the following: