Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
PolyMirae Moplen 341R Injection Molding Grade Polypropylene Moplen RP341R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP341R is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
PolyMirae Moplen RP340R Injection Molding Grade Polypropylene Moplen RP340R is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340R is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene Moplen RP343N is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP343N is a random copolymer particularly suitable for injecti.. |
|||
Flexural Modulus | 1.27 - 1.76 GPa | 185 - 256 ksi | Average value: 1.47 GPa Grade Count:5 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Hyosung Topilene J340F PP J340F Film Grade Impact CopolymerApplications: Retort CPPCharacteristics:ProcessabilityHigh impactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Hyosung Topilene J351F PP J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Hyosung Topilene J740 PP J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation.. |
|||
Flexural Modulus | 1.27 GPa @Thickness 6.40 mm |
185 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL EI5002L PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D760 |
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
LG Chemical SEETEC PB283 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
LG Chemical SEETEC PH162 HDPE Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® PM202 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvant meet their respective FDA regulations and 21 CFR 177.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM850 Polypropylene impact copolymer Titanpro® SM850 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® SM950 Polypropylene impact copolymer Titanpro® SM950 is a nucleated extra high flow material. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The.. |
|||
Flexural Modulus | 1.27 GPa @Thickness 6.40 mm |
185 ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | |
Shinil Chemical SHINCON PMMA Electro Conductive Polymer SHINCON is the product line of SHINIL's electrically conductive compound which is able to dissipate the electrostatic charge (ESD) effectively. Shinil has developed SHINCON products using Shinil's .. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | |
Shinil Chemical SHINSTRA PA-66 Devlop Structural Polymer Window Strip SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Samyang Trilen® 9550AC Polypropylene, General Purpose Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | 0.079 in/min; ISO 178 |
ExxonMobil PP7555KNE2 Polypropylene Impact Copolymer Product Description: A high melt flow rate medium impact copolymer resin designed for thin wall injection molding requiring fast cycle time and low odor.Availability: Asia Pacific Features:Good Mol.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7694E2 Impact Copolymer Product Description: A high crystallinity, medium impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for applications requiring long-term heat-agi.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (2.5 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
Asia Technology Pioneers CAP 501 PP Nanocomposite Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Flexural Modulus | 1.27 GPa | 185 ksi | ASTM D790 |
SCG Chemicals EL-Lene™ H6140B High Density Polyethylene Blow Molding Key Characteristics:Good processabilityHigh stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthExcellent appearanceOdorlessSafe for food contactGood pri.. |
|||
Flexural Modulus | 1.27 GPa | 184 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |
|||
Flexural Modulus | 1.27 - 15.0 GPa | 184 - 2180 ksi | Average value: 6.70 GPa Grade Count:6 |
Overview of materials for Thermoset Polyurethane Foam, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Glass Filled". Each property range of values reported is minimum and maximu.. |