Material Notes:
HJ740 High Isostatic PP Impact CopolymerApplications:CompoundingElectric applianceAutomobile partsCharacteristics:High stiffnessHeat resistanceMedium impactInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
ASTM D792
Melt Flow 30 g/10 min
30 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 90
90
ASTM D785
Tensile Strength, Yield 30.4 MPa
4410 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.72 GPa
249 ksi
ASTM D790
Izod Impact, Unnotched 0.637 J/cm
1.19 ft-lb/in
ASTM D256
0.343 J/cm

@Temperature -10.0 °C
0.643 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 130 °C
266 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525
Users viewing this material also viewed the following: