IPB Veralite® 100AR Antireflective Transparent APET Sheet

Category Polymer , Thermoplastic , Polyester, TP
Manufacturer IPB
Trade Name Veralite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IPB Veralite® 100AR Antireflective Transparent APET Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Antireflective has one matte surface and improved scratch resistance over Veralite®100. Used in display applications such as kiosks, POP displays, signage. It posses these attributes:excellent impact resistancehigh transparencysuperior rigidityexcellent fire ratingsfast processing (cold/hot bending)printable with recommended inksInformation provided by IPB Plastic Sheet Extrusion.
Physical Properties Metric English Comments
Density 1.33 g/cc
0.0480 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength 53.5 MPa
7760 psi
ISO 527
Elongation at Break >= 100 %
>= 100 %
ISO 527
Tensile Modulus 2.60 GPa
377 ksi
ISO 527
Izod Impact, Notched (ISO) 3.90 kJ/m²
1.86 ft-lb/in²
ISO 180
Izod Impact, Unnotched (ISO) NB
NB
ISO 180
Optical Properties Metric English Comments
Transmission, Visible 89 %
89 %
ASTM D1003