Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IRPC Polimaxx Polene 1126NK Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1126NK Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN HIGH SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: TUBULAR BLOW FILM WATER QUENCH FOR GENERAL PURPOSE FILM, FOOD AND PACKAGING BAGS, GARMENT BAGS
Physical Properties Metric English Comments
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Yield 29 %
29 %
ASTM D638
Flexural Modulus 1.45 GPa
210 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.300 J/cm²

@Temperature 23.0 °C
1.43 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 100 °C
212 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 180 - 220 °C
356 - 428 °F