ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Devcon
Trade Name Metal Welder™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Devcon Metal Welderâ„¢ Methacrylate Adhesive II, Grey / Beads.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by ITW Devcon
Physical Properties Metric English Comments
Viscosity 90000 cP
90000 cP
Mixed Viscosity (Thixotropic gel)
Mechanical Properties Metric English Comments
Elongation at Break 50 - 70 %
50 - 70 %
Adhesive Bond Strength 17.97 MPa
2607 psi
lap shear; ASTM D1002
Tensile Impact Strength >= 42.0 kJ/m²
>= 20.0 ft-lb/in²
Peel Strength 5.26 - 7.01 kN/m
30.0 - 40.0 pli
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
dry
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
dry
Processing Properties Metric English Comments
Cure Time 12.0 - 14.0 min
0.200 - 0.233 hour
Working time
55.0 - 65.0 min
0.917 - 1.08 hour
Fixture time
240 min
4.00 hour
Functional cure
Descriptive Properties Value Comments
Mix ratio (Resin:Hardener) 10:1