Indium Corp. Indalloy 100 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy , Tin Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 100 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.40 g/cc
0.303 lb/in³
Thermal Properties Metric English Comments
Melting Point 178 - 182 °C
352 - 360 °F
Solidus 178 °C
352 °F
Liquidus 182 °C
360 °F
Component Elements Properties Metric English Comments
Lead, Pb 37 %
37 %
Silver, Ag 0.40 %
0.40 %
Tin, Sn 62.6 %
62.6 %