Indium Corp. Indalloy 17 Low Melting Bismuth Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 17 Low Melting Bismuth Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.01 g/cc
0.326 lb/in³
Thermal Properties Metric English Comments
Melting Point 54.0 - 56.0 °C
129 - 133 °F
Solidus 54.0 °C
129 °F
Liquidus 56.0 °C
133 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 49.1 %
49.1 %
Cadmium, Cd 0.50 %
0.50 %
Indium, In 20.9 %
20.9 %
Lead, Pb 17.9 %
17.9 %
Tin, Sn 11.6 %
11.6 %