Indium Corp. Indalloy 191 Aluminum Solder Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 191 Aluminum Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 2.69 g/cc
0.0972 lb/in³
Thermal Properties Metric English Comments
Melting Point 577 - 630 °C
1070 - 1170 °F
Solidus 577 °C
1070 °F
Liquidus 630 °C
1170 °F
Component Elements Properties Metric English Comments
Aluminum, Al 95 %
95 %
Silicon, Si 5.0 %
5.0 %
Users viewing this material also viewed the following: