Indium Corp. Indalloy 193 Silver Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 193 Silver Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.01 g/cc
0.3616 lb/in³
Thermal Properties Metric English Comments
Melting Point 780 °C
1440 °F
Eutectic
Solidus 780 °C
1440 °F
Liquidus 780 °C
1440 °F
Component Elements Properties Metric English Comments
Copper, Cu 28 %
28 %
Silver, Ag 72 %
72 %