Indium Corp. Indalloy 221 Silver Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 221 Silver Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.71 g/cc
0.351 lb/in³
Thermal Properties Metric English Comments
Melting Point 690 - 800 °C
1270 - 1470 °F
Solidus 690 °C
1270 °F
Liquidus 800 °C
1470 °F
Component Elements Properties Metric English Comments
Copper, Cu 28.5 %
28.5 %
Nickel, Ni 2.5 %
2.5 %
Silver, Ag 63 %
63 %
Tin, Sn 6.0 %
6.0 %