Indium Corp. Indalloy 33 Bismuth Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 33 Bismuth Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.21 g/cc
0.3689 lb/in³
Thermal Properties Metric English Comments
Melting Point 87.0 - 91.0 °C
189 - 196 °F
Solidus 87.0 °C
189 °F
Liquidus 91.0 °C
196 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 51.1 %
51.1 %
Cadmium, Cd 8.1 %
8.1 %
Indium, In 1.0 %
1.0 %
Lead, Pb 39.8 %
39.8 %