Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.59 g/cc
0.346 lb/in³
Thermal Properties Metric English Comments
Melting Point 95.0 - 108 °C
203 - 226 °F
Solidus 95.0 °C
203 °F
Liquidus 108 °C
226 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 46 %
46 %
Lead, Pb 34 %
34 %
Tin, Sn 20 %
20 %