Material Notes:
Also known as 230Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.06 g/cc
0.291 lb/in³
Thermal Properties Metric English Comments
Melting Point 140 - 152 °C
284 - 306 °F
Solidus 140 °C
284 °F
Liquidus 152 °C
306 °F
Component Elements Properties Metric English Comments
Indium, In 20 %
20 %
Lead, Pb 26 %
26 %
Tin, Sn 54 %
54 %