Indium Corp. Indalloy® 60 Ga-In Eutectic Alloy for Mercury Replacement

Category Metal , Nonferrous Metal , Gallium Alloy , Indium Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy® 60 Ga-In Eutectic Alloy for Mercury Replacement.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alloy liquid at room temperature, wets glass and quartz. Mercury replacement.Information provided by the manufacturer, Indium Corporation.
Physical Properties Metric English Comments
Density 6.35 g/cc
0.229 lb/in³
Thermal Properties Metric English Comments
Melting Point 16.0 °C
60.8 °F
Eutectic
Solidus 16.0 °C
60.8 °F
Liquidus 16.0 °C
60.8 °F
Component Elements Properties Metric English Comments
Gallium, Ga 75.5 %
75.5 %
Indium, In 24.5 %
24.5 %