Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 65 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.74 g/cc
0.352 lb/in³
Mechanical Properties Metric English Comments
Elongation at Break 46 %
46 %
Thermal Properties Metric English Comments
Melting Point 70.0 - 123 °C
158 - 253 °F
Solidus 70.0 °C
158 °F
Liquidus 123 °C
253 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 30.7 %
30.7 %
Cadmium, Cd 5.1 %
5.1 %
Lead, Pb 46 %
46 %
Tin, Sn 18.2 %
18.2 %