Indium Corp. Indalloy 68 Bismuth-Lead-Tin Solder Alloy

Category Metal , Nonferrous Metal , Bismuth Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 68 Bismuth-Lead-Tin Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.48 g/cc
0.342 lb/in³
Thermal Properties Metric English Comments
Melting Point 93.0 - 127 °C
199 - 261 °F
Solidus 93.0 °C
199 °F
Liquidus 127 °C
261 °F
Component Elements Properties Metric English Comments
Bismuth, Bi 37 %
37 %
Lead, Pb 38 %
38 %
Tin, Sn 25 %
25 %