Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service

Category Metal , Ferrous Metal , Carbon Steel , Medium Carbon Steel
Manufacturer Groupe Arcelor
Trade Name SUPERELSO®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Superelso® 500 HR (SE 500 HR, "Hydrogen Resistant") is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment operating under sour service condition. It is designed to meet the requirements of NACE Standard MR0175, with a maximum hardness of 22 HRC in the heat-affected zone (HAZ) after post weld heat treatment (PWHT). SE 500 HR is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean steel. The use of special steelmaking practice imparting high steel cleanliness, along with a carefully adapted chemistry and a uniform structure provides SE500 HR with excellent resistance to wet H2S cracking, including SSC, HIC and SOHIC. The low carbon content of SE500 HR limits the HAZ hardness after welding and also improves weldability. This steel displays excellent toughness, with a low transition temperature (-60°C/-76°F). This steel is particularly suitable for pressure equipment in wet hydrogen sulfide service in the offshore oil and gas industry, where its high strength allows significant weight and cost reductions.Mechanical properties for 50-150 mm plates.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 590 - 770 MPa
85600 - 112000 psi
Typical
Tensile Strength, Yield >= 480 MPa

@Strain 0.200 %
>= 69600 psi

@Strain 0.200 %
Elongation at Break 17 %
17 %
Typical
Charpy Impact >= 50.0 J

@Temperature >=-60.0 °C
>= 36.9 ft-lb

@Temperature >=-76.0 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.10 %
<= 0.10 %
Iron, Fe 95.99 - 100 %
95.99 - 100 %
As remainder
Manganese, Mn <= 2.0 %
<= 2.0 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Nickel, Ni <= 1.0 %
<= 1.0 %
Phosphorous, P <= 0.0080 %
<= 0.0080 %
Silicon, Si <= 0.40 %
<= 0.40 %
Sulfur, S <= 0.0020 %
<= 0.0020 %