Material Notes:
Key Features:UnfilledHigh impact or high impact modifiedSuitable processing methods:Sheet extrusionThermoforming
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
Melt Flow 5.2 g/10 min

@Load 10.0 kg,
Temperature 220 °C
5.2 g/10 min

@Load 22.0 lb,
Temperature 428 °F
cm³/10 min.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.0 MPa
5370 psi
Elongation at Break 29 %
29 %
Nominal
Elongation at Yield 3.4 %
3.4 %
Tensile Modulus 1.91 GPa
277 ksi
Charpy Impact, Notched 4.10 J/cm²
19.5 ft-lb/in²
3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 94.0 µm/m-°C

@Temperature 20.0 °C
52.2 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °C
198 °F
Deflection Temperature at 1.8 MPa (264 psi) 79.0 °C
174 °F
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL Recognized
HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
UL Recognized
Electrical Properties Metric English Comments
Dissipation Factor 0.0121

@Frequency 1e+6 Hz
0.0121

@Frequency 1e+6 Hz
0.0122

@Frequency 100 Hz
0.0122

@Frequency 100 Hz
Processing Properties Metric English Comments
Melt Temperature 250 °C
482 °F
Injection Molding
Mold Temperature 60.0 °C
140 °F
Injection Molding
Injection Velocity 200 mm/sec
7.87 in/sec
Injection Pressure 55.0 MPa
7980 psi