Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS (Asia Pacific) UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*4 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CX3222ME PC+ABS Cycoloy* resin grade CX3222ME is an extrudable & thermoformable PC/ABS blend with non brominated and non chlorinated flame retardant systems. Key features of low gloss and good impact make it ideal .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® XCY630 PC+ABS (Asia Pacific) PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 940A PC (Europe-Africa-Middle East) LEXAN 940A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics Lexan® 943A PC (Europe-Africa-Middle East) LEXAN 943A is a medium viscosity flame retardant, UV-stabilized grade. UL-94 V0 listed and available in transparent and tints. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CU1650 PC+ABS UV stabilized, non-FR PC/ABS of excellent flow and impact performance |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® CFR9712 PC COPOLYMER (Asia Pacific) Lexan* CFR9712 Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 2.0 mm and high flow capability. .. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX1231T PC Copolymer (Asia Pacific) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Lexan® SLX2271T PC Copolymer (Europe-Africa-Middle East) Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colors |
|||
Charpy Impact, Notched | 3.00 - 3.00 J/cm² @Temperature -20.0 - -20.0 °C |
14.3 - 14.3 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 3.00 J/cm² Grade Count:1 |
Overview of materials for High Density Polyethylene (HDPE), Ultra High Molecular Weight This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Ultra High Molecular Weight". Each property range of values reported i.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -20.0 °C |
14.3 ft-lb/in² @Temperature -4.00 °F |
DIN 53453 |
Global PP-2800-J Polypropylene Block Copolymer Description-opacity, medium to high stiffness, high impact strength at low temperatureApplications-automotive (interior & exterior), cratesInformation provided by Global Polymers Corporation. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO Data |
Styron CALIBRE™ 891 20 Polycarbonate, General Purpose CALIBRE® 890 series polycarbonate resins are a general purpose, superior ignition resistant grade equipped with a mold release package. The CALIBRE 890 series resins exhibit a high heat resistanc.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eA |
Styron EMERGEâ„¢ 7500 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS) EMERGEâ„¢ PC/ABS 7500 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/2C |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | dry; ISO 179/1eA |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eU |
DSM Stanyl® TW371 (COND) Nylon 46 Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® TSGL-40/4 nat PA666-GF40 Product description: Grilon TSGL-40/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 natural is characterized by the following .. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® XE 5107 (GVL-5H V0) PA*-GF50 Product description: Grivory XE 5107 black 9915 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide. The product is flame retarded and reinf.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | conditioned; ISO 179/1eA |
EMS-Grivory Grivory® BGZ-30 PA6-GF30 Product description: Grilon BGZ-30 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 30% glass fibers. Grilon BGZ-30 has the following important properties:.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature 30.0 °C |
14.3 ft-lb/in² @Temperature 86.0 °F |
dry; ISO 179/1eU |
EMS-Grivory Grivory® GVL-5H black 9915 PA*-GF50 Product description: Grivory GVL-5H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H blac.. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Conditioned) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3WG6 BK00564 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 BK00564 is a 30% glass fiber reinforced, pigmented black, heat stabilized injection molding PA6 grade. |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | |
Polimeri Europa SINKRAL D720 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-08-35-15 High impact injection moulding grade, with improved flow compared with SINKRAL B620 and a high glo.. |
|||
Charpy Impact, Notched | 3.00 J/cm² @Temperature -30.0 °C |
14.3 ft-lb/in² @Temperature -22.0 °F |
Edgew 80*10*3 sp=62mm; ISO 179/1eA |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS (Asia Pacific) Cycoloy Medium Heat Plating Grade for Automotive |
|||
Charpy Impact, Notched | 3.00 J/cm² | 14.3 ft-lb/in² | ISO 179/1eA |
BASF Ultramid® B3WG6 30% Glass Filled PA6 (Conditioned) Ultramid B3WG6 is a 30% glass fiber reinforced, heat stabilized injection molding PA6 grade. |