Ineos H12E-00 Polypropylene Homopolymer, Antistatic

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H12E-00 Polypropylene Homopolymer, Antistatic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An antistated polypropylene homopolymer produced by Ineos utilizing catalyst technology.It is designed for injection molding and general purpose extrusion. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength, Yield 36.5 MPa
5290 psi
2 in/min; ASTM D638
Elongation at Yield 11.5 %
11.5 %
2 in/min.; ASTM D638
Flexural Modulus 1.558 GPa
226.0 ksi
Secant @ 1% strain at 0.05 in/min; ASTM D790
Izod Impact, Notched 0.187 J/cm
0.350 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Injection/Extrusion
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution