Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 75 LL General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CA - 75 UVT General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 81 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 82 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 82 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 86 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 75 HID General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 80 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 86 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Temperature 23.0 °C |
0.350 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ovation Polymers Nemcon™ H ES DP110/X3 Polycarbonate Alloy Polycarbonate alloy-Thermally conducting, electrically insulating grade with high HDT and improved processability.Information provided by Ovation Polymers |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers NPS 80-0201 Crystal Polystyrene Description: Injection Molding Grade, High Heat ResistantInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 75 LL General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 75 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 81 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 82 UVA General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | 0.125 in; ASTM D256 |
M. Holland Company GS411 Polystyrene
(discontinued **) Features: Good Crack Resistance, Crystal, Fast Cycle (Production), Good FlowUses: Disposable Drinkware, Electrical/Electronic ApplicationsApprovals: FDA 21 CFR 177.1640 Processing Method: Extrusio.. |
|||
Izod Impact, Notched | 0.187 - 0.694 J/cm | 0.350 - 1.30 ft-lb/in | Average value: 0.388 J/cm Grade Count:4 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | ASTM D256 |
Ineos H12E-00 Polypropylene Homopolymer, Antistatic An antistated polypropylene homopolymer produced by Ineos utilizing catalyst technology.It is designed for injection molding and general purpose extrusion. This material meets the Food and Drug Adm.. |
|||
Izod Impact, Notched | 0.187 - 0.320 J/cm @Temperature 23.0 °C |
0.350 - 0.600 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Ineos H20Z-03 Polypropylene Homopolymer This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520... |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | ASTM D256 |
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o.. |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | ASTM D256 |
Chase Plastics CP Pryme® PPH100-12M Polypropylene Homopolymer Information provided by Chase Plastics. |
|||
Izod Impact, Notched | 0.187 J/cm | 0.350 ft-lb/in | 1/8 in.; ASTM D256 |
Chevron Phillips MC3700 High Flow Crystal Polystyrene DescriptionChevron polystyrene resin MC3700 crystal is a free-flowing, crystal clear polystyrene injection molding compound, designed specifically for thin- and medium-walled or long-flow, difficult.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 75 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 75 HID General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 75 UVA General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite Optix® CP - 80 General Purpose Acrylic Resin OPTIX® general purpose acrylics are available in a variety of performance grades that offer varying melt flow rates, heat resistance, color/opacity and gloss levels.Information provided by Plaskoli.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CA - 75 UVT General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 75 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |
|||
Izod Impact, Notched | 0.187 J/cm @Thickness 6.35 mm |
0.350 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Plaskolite West Optix® CP - 82 General Purpose Acrylic Resin Generally unaffected by alkalis, hydrocarbons, non-oxidizing acids, and salt water. Transparent, translucent, opaque, and custom colors in various grades of melt flow rate and heat resistance are av.. |