Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H36G-01 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Fiber Grade , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H36G-01 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a polypropylene homopolymer for general purpose injection molding and high speed fiber spinning applications. It is useful for spunbonded nonwovens and partially oriented yarn (POY). This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsSpunbond nonwovensPOYFiber and tapeGeneral purpose injection moldingStaple fiberBenefitsExcellent gas fadeExcellent processabilityHigh speed spinningInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 36 g/10 min

@Load 2.16 kg,
Temperature 230 °C
36 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 32.1 MPa

@Temperature 23.0 °C
4660 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 1.22 GPa

@Temperature 23.0 °C
177 ksi

@Temperature 73.4 °F
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C
198 °F
ASTM D648
Users viewing this material also viewed the following: