Material Notes:
Extrusion. Features: No Slip, Antiblock.Applications: Cast filmTypical property data below from injection molded samples.
Physical Properties Metric English Comments
Density 0.910 g/cc
0.0329 lb/in³
Typical value for polypropylene.
Melt Flow 7.3 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.3 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 38.0 MPa
5510 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648