Ineos L80Z-00 Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos L80Z-00 Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
L80Z-000 impact copolymer polypropylene is a high melt flow rate, nucleated and antistatic grade designed for high-speed injection molding applications. This resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:Thin-wall injection molding applications (TWIM)Housewares, consumer goods including storage container & lidsAudio-video media packaging formats (DVD & CD cases)Cups, containers and related rigid packagingBenefits:Easy mold fillingVery good impact-to-stiffness balanceFast cycling / Excellent overall processabilityGood mold release and static charge dissipationInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 230 °C
80 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 79
79
ASTM D785
Tensile Strength, Yield 23.35 MPa
3387 psi
ASTM D638
Flexural Modulus 1.19 GPa
172 ksi
ASTM D790A
Izod Impact, Notched 0.625 J/cm

@Temperature -20.0 °C
1.17 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
1.28 J/cm

@Temperature 23.0 °C
2.40 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 101.7 °C
215.1 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution