Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched = 1.28 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched 1.28 J/cm

@Temperature -30.0 °C
2.40 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 1.28 J/cm

@Temperature -30.0 °C
2.40 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 1.28 J/cm

@Temperature -30.0 °C
2.40 ft-lb/in

@Temperature -22.0 °F
ASTM D 256
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
Izod Impact, Notched 1.28 J/cm

@Thickness 3.20 mm,
Temperature -30.0 °C
2.40 ft-lb/in

@Thickness 0.126 in,
Temperature -22.0 °F
ASTM-D256
Ineos ABS Lustran® 720 ABS, Molding Grade
Lustran® ABS 720 resin is a black, virgin injection molding grade of ABS (acrylonitrile butadiene styrene). It is supplied as salt-and-pepper pellets with color concentrate 901802 black. Designed..
Izod Impact, Notched 1.28 J/cm

@Temperature 23.0 °C
2.40 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Ineos L80Z-00 Impact Copolymer Polypropylene
L80Z-000 impact copolymer polypropylene is a high melt flow rate, nucleated and antistatic grade designed for high-speed injection molding applications. This resin meets the requirements of the U.S...
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm,
Temperature -40.0 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature -40.0 °F
ASTM D256
Techmer ES Elastoblend® PA6 GF40 IM2 NAT 40% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedUL File Number: E157318Processing Meth..
Izod Impact, Notched 1.28 J/cm

@Thickness 6.35 mm
2.40 ft-lb/in

@Thickness 0.250 in
TPI Porene® ABS-AN450 Flame Retardant ABS Resin
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm,
Temperature -18.0 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature -0.400 °F
ASTM D256
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES
Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can..
Izod Impact, Notched 1.28 J/cm

@Temperature 23.0 °C
2.40 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D256
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612
Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Notched 1.28 J/cm

@Thickness 3.17 mm,
Temperature 22.8 °C
2.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.0 °F
ASTM D256
Techmer ES Plastiblend® ABS/PA 1700
Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc.
Copyright © lookpolymers.com All Rights Reserved