Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 1-3830 30% Glass-Fiber-Filled Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 1-3830 is a 30% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3830 is recommended for producing injection molded products, where the required properties are high strength and stiffness.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 1.13 g/cc

@Temperature 23.0 °C
0.0408 lb/in³

@Temperature 73.4 °F
ISO 1183
Linear Mold Shrinkage 0.0080 - 0.016 cm/cm
0.0080 - 0.016 in/in
ISO 294-4:1997
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 3.2 %
3.2 %
50 mm/min; ISO 527-1,-2
Tensile Modulus 5.00 GPa
725 ksi
ISO 527-1,-2
Flexural Modulus 4.80 GPa
696 ksi
2 mm/min; ISO 178
Charpy Impact, Notched 0.550 J/cm²

@Temperature -20.0 °C
2.62 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
0.700 J/cm²

@Temperature 23.0 °C
3.33 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 155 °C
311 °F
ISO 75-1,-2
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
FMVSS 302
Descriptive Properties Value Comments
Automotive Materials Pass
FMVSS 302
Color Natural