Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVAMID® 6/66 GF 15 GB 15 PA6/66 reinforced with glass fiber, glass beads PA 6 and PA 66 alloy for injection molding, reinforced with 15% glass fiber and 15 % glass beads, for moldings used in the automotive, electrical, building, engineering and hobby industry - holders .. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179 |
Polykemi AB SCANBLEND P AP2060 F20 PBT/ASA, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S CP400 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
PolyOne Bergamid™ A70 G35 H U BK SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on polymer only) with low warpage and superior strength, stiffness and sur.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® 45HSB NC010 Nylon 66
(Unverified Data**) Zytel® 45HSB NC010 is a high viscosity, heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Minlon® 73GM40 NC010 Nylon 6
(Unverified Data**) Minlon® 73GM40 NC010 is a 40% mineral/glass reinforced, heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Inno-Comp INNOPOL® CS 1-3830 30% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-3830 is a 30% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3830 is recommended for producing in.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
|
LATI Larton GCE/600 PPS, Glass/Mineral Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers / Mineral filler. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa .. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
|
LATI Latilon 28D G/20 PC, 20% Glass Fiber Reinforced Polycarbonate (PC) based compound. Glass fibers. Low smoke density and low toxicity index. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North A.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
Sax Polymers SAXAMID 226F4RY01 Nylon 6.6, 20% Glass Fiber SAXAMID 226F4RY01 is a polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers. It has a halogen-free flame retardant.Information provided by SAX Polymers |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EF210AE Polypropylene TPO Compound Daplen™ EF210AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Unipetrol PE HD LITEN® FB 85 HDPE Made for tubular film applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® S1320 003 POM Description: Is a POM, free-flowing, rapidly solidifying grade for moldings difficult to produce by injection molding and having low wall thicknesses, higher stiffness and thermal stability.Informat.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eA |
BASF Ultramid® B3WGM 24 HP BK 23210 10/20% Glass/Mineral Filled PA6-1 (Dry) Description: 20% mineral-filled and 10% glass-fiber reinforced injection-molding grade with outstanding flowability for technical parts with medium rigidity and high dimensional stability, e.g. for.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
DAM; ISO 179/1eA |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Zytel® FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applications such as parts for the food industry.Information provided by D.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Ascend Performance Materials Vydyne® 50BWFS Nylon 66, Dry as Molded Vydyne® 50BWFS is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a highviscosity resin. This resin offers a well-balanced com.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -30.0 °C |
2.62 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Unipetrol PE HD LITEN® MB/ML 71 HDPE Made for injection molding applications.Information provided by Unipetrol RPA |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature -20.0 °C |
2.62 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eA |
Borealis Daplen™ EF209AE Polypropylene TPO Compound Daplen™ EF209AE is a 20% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Charpy Impact, Notched | 0.550 J/cm² @Temperature 23.0 °C |
2.62 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |