Invista 3302 PET Copolymer Packaging Resin  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Invista 3302 PET Copolymer Packaging Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Carboxyl end groups:
Physical Properties Metric English Comments
Bulk Density 0.830 g/cc
0.0300 lb/in³
Density >= 1.39 g/cc
>= 0.0502 lb/in³
HC No. 300 test
Viscosity Measurement 0.77 - 0.82
0.77 - 0.82
Intrinsic viscosity; WI No. 104 test; correlated from solution viscosity by Invista
Thermal Properties Metric English Comments
Melting Point >= 246 °C
>= 475 °F
HC No. 72A test
Descriptive Properties Value Comments
Process Blow Molding
Injection Molding