Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0300 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.830 g/cc
0.0300 lb/in³
Tapped
Nyco NYAD® 5000 Wollastonite
Fine particle size grade. This grade is recommended for polymer reinforcement.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distincti..
Bulk Density 0.830 g/cc
0.0300 lb/in³
Poured; ASTM D1895
Eastman A12 PET  (discontinued **)
Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i..
Bulk Density 0.830 g/cc
0.0300 lb/in³
Poured; ASTM D1895
Eastman CB11E PET  (discontinued **)
VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet..
Bulk Density 0.830 g/cc
0.0300 lb/in³
Invista 1101 PET Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups:
Bulk Density 0.830 g/cc
0.0300 lb/in³
Invista 3301 PET Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups:
Bulk Density 0.830 g/cc
0.0300 lb/in³
Invista 3302 PET Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups:
Bulk Density 0.830 g/cc
0.0300 lb/in³
ISO 60
FKuR Kunststoff Bio-Flex® F 1130 Compostable PLA Blend
The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D1895
Plenco 1500 Polyester, Granular, Compression Molded
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under compon..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D1895
Plenco 1581 Polyester, Pellet, Injection Molded
PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D1895
Plenco 7556 Phenolic, Briquette, Transfer Molded
PLENCO 07556 is a glass fiber reinforced novolac phenolic molding compound, with good physical strengths and heat resistance along with excellent dimensional stability. UL recognized under component..
Bulk Density 0.830 g/cc
0.0300 lb/in³
DuPont™ Nomex® N196 Paper, 20 mil Nominal Thickness
Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili..
Bulk Density 0.830 g/cc
0.0300 lb/in³
Daikin NEOFLON AC-5820 PFA Coating Powder, White
NEOFLON PFA coating powder is designed for high build coatings having excellent resistance to chemical and corrosive environments.Description: 0.5-5 mm thickness.Processing Methods: Electrostatic sp..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894-98a
3M Dyneon™ TFM™ 1600 PTFE
Meets ASTM D4894 Type III, Grade 2 resinMolding and ram extrusion powder with very good free flowing propertiesGood metering propertiesGood mold filling behaviorImproved particle coalescenceDenser p..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894-98a
3M Dyneon™ TF 1641 PTFE
Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesVery ..
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D4894-98a
3M Dyneon™ TF 1645 PTFE
Meets ASTM D4894 Type IV, Grade 2 resinMolding and ram extrusion powder very good free-flow propertiesGood metering propertiesGood mold filling behaviorGood electrical and mechanical propertiesUsed ..
Bulk Density >= 0.830 g/cc
>= 0.0300 lb/in³
Pycnometer test
Invista 1101R Copolymer Packaging Resin  (discontinued **)
Carboxyl end groups:
Copyright © lookpolymers.com All Rights Reserved