Iran Petrochemical (PCC) GPPS 1160 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Extrusion Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) GPPS 1160 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GPPS 1160 is a high heat resistance, high molecular weight crystalline polystyrene used in the extrusion industry. It is most suitable for production of oriented polystyrene. It is particularly useful for production of thick sheet by direct gassing, where it gives expanded sheets with high mechanical properties.Applications: shower cabinets; lighting thin films; thermoforming, transparent cups, insulation board, foamed sheetInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
Moisture Absorption <= 0.100 %
<= 0.100 %
ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D570
Melt Flow 2.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
2.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 3.20 GPa
464 ksi
ASTM D638
Flexural Modulus 2.90 GPa
421 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point >= 101 °C
>= 214 °F
ASTM D1525
Optical Properties Metric English Comments
Refractive Index 1.591
1.591
ISO
Transmission, Visible 90 %
90 %
transparent; thickness not quantified