Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antistatic properties.Applications: cast film and water quenched blown film, laminationInformation provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ISO 1183
Melt Flow 8.0 g/10 min
8.0 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ISO 868
Tensile Stress 28.0 MPa
4060 psi
ISO R527
Elongation at Yield 14 %
14 %
ISO R527
Flexural Modulus 1.05 GPa
152 ksi
ISO 178
Izod Impact, Notched (ISO) 4.50 kJ/m²
2.14 ft-lb/in²
ISO 180