Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.05 GPa | 152 ksi | STN EN ISO 178 |
Plastcom PLASTALEN® PQ 82 N Polypropylene with improved impact strength PP impact modified. General application in all industry branches. Delivered in natural mode and in the full RAL color scale. For injection molding.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP FR 7B31 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 1365S (H22S) Propylene Homopolymer Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P.. |
|||
Flexural Modulus | >= 1.05 GPa | >= 152 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PP 4215M (EP1X35F) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
FKuR Kunststoff Bio-Flex® F 2201 CL Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9302 Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9302 is an elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9302 is developed for produ.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 2% secant; ASTM D790-02 |
Ipiranga Petrochem HC 7260 LS HDPE IPQ produces High Density Polyethylene (HDPE) for use by different segments of the plastics molding industry in several processes, including blow molding, extrusion and injection molding.To produce .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Iran Petrochemical (PCC) 5218EA High Density Polyethylene HD-5218EA is a high density polyethylene copolymers containing butane-1 as the comonomer with narrow molecular weight distribution, suitable for thin wall injection application. It has been designed.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Iran Petrochemical (PCC) EPD 60 R Polypropylene EPD 60 R has a high molecular weight giving it superior toughness even at low temperature. It has excellent heat and detergent resistance.Applications: extrusion blow molding applications include t.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Iran Petrochemical (PCC) Moplen EP1 X 35 AF Polypropylene Moplen EP1 X 35 AF is a slightly modified random copolymer for the production of cast and water-quenched blown film. It is formulated with a slip and antiblock package and exhibits excellent antist.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D760-66 |
Micropol Microlin ML27 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | |
Kraton® D1102 + PP blend (25/75) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | |
Kraton® G1652 + PP blend (10/90) Unmodified polypropylene has high rigidity and good heat resistance, but poor impact resistance, especially at low temperatures. Blending KRATON D and G polymers with PP significantly improves the .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600T10-BK TPO, 10% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
MRC Polymers MAXTELâ„¢ 600-BK TPO, Black For automotive exterior applications. Excellent process ability and dimensional stability.Unfilled TPOAvailable in black and gray onlyCan be UV StabilizedInternal and external lubricants can be add.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178-1975 |
SIDPEC EGYPTENE® HD 5218 EA HDPE Injection Molding Applications:House waresThin-walled food containersPET bottle base cupInformation provided by Interchim s.r.l., official distributor of Sidi Kerir Petrochemicals Co. (SIDPEC) Products |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1mm/min; ISO 178 |
Borealis BL1481 High Density Polyethylene BL1481 is a semi high molecular weight polyethylene comprising an extra ordinary ESCR and very good chemical resistance This product is intended for blow molding. This grade is available in granular.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EE040AE TPO Compound Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | At 2 mm/min; ISO 178 |
Borealis Daplen™ EF040AE TPO Compound Daplen EF040AE is a elastomer modified polypropylene compound intended for injection molding. Daplen EF040AE is a material with excellent impact/stiffness ratio. Thanks to its low thermal expansio.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PE HD LITEN® BB 29 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 935 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 950 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 805 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Unipetrol PP MONSTEN® MT 812 Polypropylene Random Copolymer Made for injection molding applications. Antistatic and transparent stabilization. Random copolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Chengdu Polyster H9275Y Thermoplastic Polyether-ester Elastomer (TPEE) High modulus molding and injection grade. Contains improved color- stable antioxidants. Excellent heat-ageing resistance and toughness. Applications requiring high strength, high toughness and good .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7035E5 Impact Copolymer Product Description: A medium impact copolymer resin designed for injection molding applications requiring high melt flow rate.Availability: North America Features:Good ColorablityGood Dimensional .. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
BASF Ultramid® HFX 35 PA6 (Dry) Description: Ultramid HFX 35 is a polyamide specialty extrusion resin combining high flexibility, outstanding chemical resistance and enhanced heat stability.Applications: Ultramid HFX 35 is recomme.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ASTM D790 |
Carmel Olefins CAPILENE® QT 73 A Propylene Random Copolymer Description: CAPILENE® QT 73 A is a clarified and antistatic additivated polypropylene random copolymer with a high melt flow rate, intended for injection molding of clear articles. It exhibits g.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF BLK Nylon 66, DAM Vydyne® 21SPF BLK is a, general-purpose PA66 resin used for extrusion-compounding. Available in black, it is designed principally for injection-molding fabrication. This grade offers a well-balance.. |
|||
Flexural Modulus | 1.05 GPa | 152 ksi | ISO 178 |
Ascend Performance Materials Vydyne® 21SPF1 Nylon 66, Conditioned Vydyne® 21SPF1 is a general-purpose PA66 resin available in natural color. It is designed principally for injection-molding applications with the added benefits of improved flow during the molding .. |