Material Notes:
Information provided by JPJ Technologies
Physical Properties Metric English Comments
Bulk Density 0.460 - 0.540 g/cc
0.0166 - 0.0195 lb/in³
Particle Size <= 350 µm
<= 350 µm
<0.1% exceeds 0.35 mm
Descriptive Properties Value Comments
Average polymerization degree 1270-1380
Fish eye <5/100 cm2
Impurity particle number <50/100g
Initial whiteness >90%
K Value 71-72
VCM residuals <1 ug/g
Whiteness >78%