Polymer Property : Bulk Density = 0.0195 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density 0.480 - 0.540 g/cc
0.0173 - 0.0195 lb/in³
PVCH/QCD/3516
Reliance Industries 57-01 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Rigid injection.
Bulk Density 0.480 - 0.540 g/cc
0.0173 - 0.0195 lb/in³
PVCH/QCD/3516
Reliance Industries 60-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications:Recommended:Rigid extrusionRigid injectionRigid calenderingCan be used:Blow molding
Bulk Density 0.480 - 0.540 g/cc
0.0173 - 0.0195 lb/in³
PVCH/QCD/3516
Reliance Industries 67-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Recommended:Flexible extrusionFlexible injectionFlexible calenderingCan be used:Rigid injectionRigid extrusion
Bulk Density 0.480 - 0.540 g/cc
0.0173 - 0.0195 lb/in³
PVCH/QCD/3516
Reliance Industries 57-11 Polyvinyl Chloride
Information provided by Reliance IndustriesApplications: Rigid injectionRigid extrusionRigid calenderingblow molding
Bulk Density 0.460 - 0.540 g/cc
0.0166 - 0.0195 lb/in³
ASTM D1895
LG Chemical LS130S PVC
General Description: LS130S, homopolymer made by suspension polymerization, is mainly used in PVC wire extrusion and calendar processing, well known for giving clean surfaces and bright color to the..
Bulk Density 0.460 - 0.540 g/cc
0.0166 - 0.0195 lb/in³
ASTM D1895
LG Chemical LS170 PVC
General Description: LS170, homopolymer made by suspension polymerization, is applied for value added products such as matted sheeting, super heat resistant wire ,high pressure hose, packing and gas..
Bulk Density 0.460 - 0.540 g/cc
0.0166 - 0.0195 lb/in³
JPJ Technologies DG-1300 PVC
Information provided by JPJ Technologies