Material Notes:
General purpose, good matching properties. Copper, cobalt, gold, iridium, palladium and ruthenium alloy easily with platinum. The differences between the alloys reflect the hardening of the alloying element itself.
Physical Properties Metric English Comments
Density 20.7 g/cc
0.748 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 130
130
Annealed
Elongation at Break 32 %
32 %
Annealed
Thermal Properties Metric English Comments
Melting Point 1780 - 1795 °C
3240 - 3263 °F
Solidus 1780 °C
3240 °F
Liquidus 1795 °C
3263 °F
Component Elements Properties Metric English Comments
Platinum, Pt 95 %
95 %
Ruthenium, Ru 5.0 %
5.0 %